High Efficiency Promised By Nozzle-Free Coating System

A coating system which elininates spray nozzles promises transfer efficiencies of 90% and improved uniformity.

Author
Un-named
Origin
Unknown
Journal Title
Glass Industry 79 5 1998 29-30