High Chrome Refractories For Severe Wear Areas In Soda-Lime Glass Melters

High chrome refractories were developed decades ago to address high wear areas in soda-lime melters. Today's field experience demonstrates very good behaviour of these high chromium oxide refractories in submerged areas after several years of use. They are now a leading choice for high pull rate soda-lime furnaces, as reported in this article.