High-Alumina Low-Silica Ht Stone Wool Fibres: A Chemical Compositional Range With High Biosolubility

Man-made vitreous fibres (MMVF) are classified within the EU as a carcinogenic category 3 (possibly carcinogenic), but criteria exist to exonerate fibers from this classification. The HT stone wool fibre type is a MMVF that fulfils EU regulatory requirements for exoneration from classification as a carcinogen based on in vivo testing. The chemical composition of the fibres and the results of the in vivo and in vitro studies that defend the chemical compositional range for a CAS registry number for these are presented and discussed.

Author
M Guldberg Et Al
Origin
Rockwool International, Denmark
Journal Title
Regulatory Toxicology & Pharmacology 35 2002 217-226
Sector
Glass Fibre
Class
GF 527

Request article (free for British Glass members)

High-Alumina Low-Silica Ht Stone Wool Fibres: A Chemical Compositional Range With High Biosolubility
Regulatory Toxicology & Pharmacology 35 2002 217-226
GF 527
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 9 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.