High Added Value Glass Products Through Wet Chemcial Coating Techniques

The modification of glass surfaces by applying thin films of inorganic oxides is an attractive means to change the physical and chemical properties of the substrate and create new business opportunities for glass manufacturers. Besides the well-established atmospheric pressure CVD and vacuum based large-scale coating facilities, sol-gel processing is still an attractive and economic alternative for smaller and medium-size substrate dimensions as well as for special market segments due to its simple application via dip coating, spin coating or spraying procedures.

Author
Un-named
Origin
Fraunhofer Inst For Silicate Research, Germany
Journal Title
Glass Coatings 1/2005 36-37
Sector
Flat glass
Class
F 1758

Request article (free for British Glass members)

High Added Value Glass Products Through Wet Chemcial Coating Techniques
Glass Coatings 1/2005 36-37
F 1758
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 10 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.