Helium Solubility In Sodium Silicate Glasses And Melts

Helium solubilities have been measured in sodium silicate glasses at 500 deg C and in melts at 1420 deg C using a saturation outgassing method. Measurements over the temperature range from =200 to 1500 deg C were made for the 20Na20.80Si02 composition. Helium solubilities in the glasses at 500 deg C and in the melts at 1420 deg C decrease with increasing concentration. The compositional dependence of helium solubility is greater in glasses than in the melts. The data for the 20Na20.80Si02 composition indicate that the solubility of helium decreases with increasing temperature for the glasses, passes through a minimum in the glass transformation range and then increases with increasing temperature for the melts. The results are discussed in terms of the effect of composition and temperature on the free volume of these materials.

Author
M G Mesko Et Al
Origin
Alfred University, New York
Journal Title
Phys Chem Glasses 41 3 2000 111-116
Sector
Special Glass
Class
S 1978

Request article (free for British Glass members)

Helium Solubility In Sodium Silicate Glasses And Melts
Phys Chem Glasses 41 3 2000 111-116
S 1978
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.