Heat Transfer In Glass Container Moulds

Various methods of optimising heat transfer in moulds are discussed.

Author
A Chaudhuri
Origin
Krishnaa Glass Ltd, India
Journal Title
Kanch 1 2 June 1992 9-16
Sector
Container glass
Class
C 509

Request article (free for British Glass members)