Heat-Resistant Coating For Is Machine Parts Developed By Wiegand-Glas

Since the beginning of 2000, the German company Wiegand-Glas has been using a special coating for its IS machine parts. This coating is called IS-Clean and was designed for highly stressed metal parts, such as neck ring holders of IS machines. IS-Clean offers these advantages: The cleaning time after a job change is reduced considerably; time-consuming sandblasting is not required; stubborn incrustations of remaining grease can be wiped off just with water. The neck ring holders and other parts can thus be prepared for the next production period during the job change and be used again immediately. For more information on the product please telephone Wiegand on +49 9263 80258.

Author
Un-named
Origin
Unknown
Journal Title
Glastech Ber Glass Sci Technol 73 11 2000 360
Sector
Container glass
Class
C 1696

Request article (free for British Glass members)

Heat-Resistant Coating For Is Machine Parts Developed By Wiegand-Glas
Glastech Ber Glass Sci Technol 73 11 2000 360
C 1696
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
14 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.