Heat-Insulating Silica Bricks: Manufacture, Properties And Applications

Increased awareness surrounding energy consumption is challenging refractory manufacturers to create products of smaller volume weight with superior heat-insulating properties. In this paper, the author describes heat-insulating silica and its application in the glass industry. Attention is paid to its history, today's product ranges and development trends in the manufacture of heat-insulating silica.

Author
M Kotoucek Et Al
Origin
P-D Refractories, Czech Republic
Journal Title
Glass International March 2012 33-34, 36, 38, 40
Sector
Refractories
Class
R 752

Request article (free for British Glass members)

Heat-Insulating Silica Bricks: Manufacture, Properties And Applications
Glass International March 2012 33-34, 36, 38, 40
R 752
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 4 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.