Heat Capacity Changes At The Glass Transition In Mixed-Alkali Tellurite Glasses

The heat capacity changes at the glass transition in mixed-alkali tellurite glasses of (20-x)Li20-xNa20-80Te02 that show different fragilities, depending on the Na20/Li20 ratio, have been measured to obtain more detailed information on the structure of tellurite glasses or supercooled liquids with a fragile character.