Harnessing The Benefits Of Refractory Ceramic Fibres

With excellent insulating and mechanical properties and good corrosion resistance, ceramic fibres are ideal materials for lining glass refractories. But the carcinogenic effects of these materials have been causing concern. This paper looks at the benefits and risks.