Hafnium Solubility Determination In Soda-Lime Aluminosilicate Glass

The solubility of hafnium dioxide (HfO2), used as a surrogate for tetravalent uranium, is measured in glass melts belonging to the CaO-Al2O3-SiO2 and Na2O-CaO-Al2O3-SiO2 systems, under oxidizing and reducing conditions. Two methods have been carried out to determine it and the kinetic factors controlling the HfO2 dissolution in glass melt have been investigated in order to approach equilibrium. The solubility ranges from 3 to 6.5 mol% HfO2 in aluminosilicate glasses at temperature between 1250 °C and 1400 °C, and is not affected by the redox conditions. Conversely, the solubility is modified by the melting temperature and the glass composition. The excess of alkalis or alkaline earths which are not involved in the charge balance of AlO4 tetrahedrons in the silica network appears to play a significant role. Glass homogeneity is checked by scanning electron microscopy and X-ray diffraction. HfO2, HfSiO4, Ca2HfSi4O12, Na4Hf2(SiO4)3 and Na2HfSi2O7 are metastable crystals observed in the glass melts. The stability of those crystalline phases mainly depends on the glass composition.

Author
P. Chevreuxa Et Al
Origin
Unknown
Journal Title
J Non-Cryst Solids 457 Feb 2017 13-24
Sector
Special Glass
Class
S 4383

Request article (free for British Glass members)

Hafnium Solubility Determination In Soda-Lime Aluminosilicate Glass
J Non-Cryst Solids 457 Feb 2017 13-24
S 4383
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
4 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.