Guidelines For The Identification Of Foreign Bodies Reported From Food (2Nd Edition)

Rapid and accurate identification of foreign body material in food is essential in order that the source of contamination can be ascertained and appropriate measures taken to handle the incident and prevent recurrence. Pinpointing the state in the food chain at which contamination took place can require skilled detective work. This document is a review of guideline methods that can be used by companies with appropriate analytical facilities, and show where help may be obtained when in-house services are not available. The publication is for use by scientists with suitable expertise, but will also be of value to managers with responsibility for quality control and quality management procedures at any point in the food chain. Advice on prevention of contamination of foods on the production line is given in CCFRA Guideline No 5: Foreign Bodies in Foods.

Author
Un-named
Origin
Unknown
Journal Title
Ccfra 2006 Guideline No 4
Sector
Container glass
Class
C 2930

Request article (free for British Glass members)

Guidelines For The Identification Of Foreign Bodies Reported From Food (2Nd Edition)
Ccfra 2006 Guideline No 4
C 2930
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.