Group Optical Basicity Of Tellurite Glasses

The group basicities, ^, of TeO4, TeO4, TeO3 groups have been determined for binary tellurite glasses in the MeO-TeO2 (Me=Mg, Sr, Ba and Pb) systems from their refractive index based optical basicity, ^(n0), and fractions of the individual groups in the glass structure. Average values of group basicities namely ^TeO4 = 1.23, ATeO4=0.99 and ^TeO3-0.82 have been proposed which can be used for prediction of optical basicity of other tellurite glasses.

Author
V Dimitrov & T Komatsu
Origin
Unknown
Journal Title
Phys. Chem. Glasses: European Journal Of Glass Science And Technology B, Vol 52, No 3, June 2011
Sector
Special Glass
Class
S 3879

Request article (free for British Glass members)

Group Optical Basicity Of Tellurite Glasses
Phys. Chem. Glasses: European Journal Of Glass Science And Technology B, Vol 52, No 3, June 2011
S 3879
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
15 + 1 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.