Grit Blasting Case Study

This paper briefly describes a project requested by HFK Industries of LA, for an analysis of blasting processes and controls at their plant located in Fujian Province, China. The project was designed to initially audit the overall blasting process and process controls, recommend possible improvements for the process, and then implement and measure gains from the improvement opportunities identified.