Grinding Of Optical Glasses With Cup Wheels - A New Way To Generate Polishable Surfaces

Results of rough grinding tests offer the possibility of eliminating the fine grinding process from the machining sequence. Surface quality, research methods and measuring techniques used in the study are described.