Graphical Statistical Analysis And Its Applications To Glass.

The expression "graphical statistical analysis" (the term "statistical" seems to be a little misleading) is used for the method of structural analysis by plotting different structure sensitive properties (density, refractive index, specific refraction (n2 - 1)/(n2+2)x(1/d), etc) vs. molecular weight or a similar factor. This method has been successfully applied to hydro carbon mixtures, and an attempt has been made to use it for glasses to obtain data on their degree of polymerization. A linear relationship exists between the specific refraction and the percentage of K2O of a potassium-silicate glass. The extrapolated value for 0% coincides exactly with the value for vitreous silica previously given. 39 figures, 29 references.

Author
Hi Waterman
Origin
Unknown
Journal Title
Silicates Ind 19 8/9 273-82 10 326-34 1954
Sector
Primary Papers
Class
PP 1374

Request article (free for British Glass members)

Graphical Statistical Analysis And Its Applications To Glass.
Silicates Ind 19 8/9 273-82 10 326-34 1954
PP 1374
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
17 + 0 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.