Gob Temperature Control Strategy

Significant quality and throughput improvements to the glass container manufacturing process have been demonstrated by a control method that directly controls the gob temperature. The method combines ACSI's predictive-adaptive model-based control system with BASF's Exactus high speed optical gob temperature sensor.

Author
Un-named
Origin
Unknown
Journal Title
Glass Worldwide Sept/Oct 2010 68
Sector
Container glass
Class
C 4230

Request article (free for British Glass members)

Gob Temperature Control Strategy
Glass Worldwide Sept/Oct 2010 68
C 4230