Gluing Of Accessories To Glass Containers

This article suggests some guidelines that should be observed during the application of a gluing assembly project. There is an evaluation of the implications coming from glass shape, glass surface and the kind of glue. The main assembly process risks are discussed, as are the control criteria for the assembled products. The aim is to stress the critical aspects linked to different steps of the assembly process, starting from the evaluation of the project needs up to the final controls of the assembled items.

Author
G Marchini
Origin
Cerve, Italy
Journal Title
Gmpa 4/09 76-77
Sector
Container glass
Class
C 3982