Glazing The Nation'S Cars

RAC Auto Windscreens is the UK's biggest supplier of replacement windscreens. The company stocks over 10,000 different vehicle windows and has to cater for a wide variety of shapes and sizes within each individual vehicle type. This article looks at how changes in the market have affected the way in which the company sources its windscreens.

Author
Un-named
Origin
Unknown
Journal Title
Glass 80 10 Nov/03 320
Sector
Flat glass
Class
F 1474