Glaze Coatings Based On Zirconium Glass With Low Boron Content

The Na20-B203-Al203-Si02-Zr02 system was chosen as the starting system to synthesize glazes for facing tiles. The optimum glass compositions contained 10-17.5 mol% B203 and 4-5 mol% Zr02. The resulting glasses had good founding and processing properties. The glass samples were specified with X-ray amorphism and small regions of phase separation. Transparent, opaque and partially opaque glasses were produced. The marjority of transparent glasses preserved no opacity even after long thermal treatment, which indicates a trend towards crsytallization. The glass structure was studied by methods of differential and thermal analysis and by infrared spectroscopy.

Author
I Levitsky & T Kolontayeva
Origin
Belarusian State University
Journal Title
Proc Xviii Icg, San Francisco, Usa, July 1998 207-212
Sector
Special Glass
Class
S 1863

Request article (free for British Glass members)

Glaze Coatings Based On Zirconium Glass With Low Boron Content
Proc Xviii Icg, San Francisco, Usa, July 1998 207-212
S 1863
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.