Glaverbel Opens In Kiln, Russia

Glaverbel has underlined its position as leader in the Russian flat glass market by opening a new manufacturing complex at Kiln, north-west of Moscow. The new plant will produce 180,000/tpa and includes two downstream processing units, one for large-scale super-insulating coated glass and another for MNGE (Mirox New Generation Ecological) mirrors.