Glassprom'91 Gateway To The East

This event is reported, based mainly on the analysis made by participants on the Soviet side.

Author
R Hamilton
Origin
Unknown
Journal Title
Glass Machinery Plants & Accessories 1991 5 4 50 - 58
Sector
General
Class
G 683