Glassmaking Raw Materials Trends In China

Chinese glassmakers have witnessed significant fluctuations in raw material prices in recent years, a situation that has posed a number of challenges. This article provides an overview of availability and pricing (in RMB/CNY) of silica sand and soda ash. For example, in 2017, the high for soda ash was in the region of RMB 2610/ton (around £300) and the low was RMB 1920/ton (around £220).

Author
Un-named
Origin
Unknown
Journal Title
Glass Worldwide 2/2018 52-54
Sector
General
Class
G 4719