Glassmaking Is A Natural Process - With Gas Chromatography

Natural gas delivers clean, high-quality energy for many industry sectors. When it is a matter of achieving consistent combustion and melting processes, as with the glass industry, the quality of the gas has a crucial influence on the process. In this article the author looks how the continuous monitoring of quality parameters, with the aid of process gas chromatographs, created the basis for optimised burner controllers.

Author
Dr S Malcharek
Origin
Siemens, Germany
Journal Title
Glass International June 2012 41-42
Sector
General
Class
G 4019