Glassmaking In The Eu Gets More Concentrated

The 25 member countries of the EU for the world's largest glass market in terms both of production and consumption. The EU glass industry consists of around 1,300 firms. It is highly concentrated with over 80% of glass produced by fewer than 10 multinational companies, each with more than 1000 employees. The other companies are small or medium-sized but mainly specialists.