Glasses And Glass-Ceramics Of The System Cao-Mg0-Al203-Si02 Obtained From Natural Sedimentary Raw Materials

Common and low-cost natural sedimentary raw materials such as ball clay, dolomite, quartz sand and diatomite were used as the main constituents for the production of glasses and glass-ceramics of the system SaO-MgO-Al203-Si02.