Glass Transition Phenomena And Cation Vibrations In Alkali Borate Glasses

The effect on the glass transition temperature of the interactions between alkali cations and the glass network in binary alkali glasses has been investigated.

Author
E I Kamitsos, G D Chyrssikos, M A Karaksiddes
Origin
National Hellenic Research Foundation
Journal Title
Physics And Chemistry Of Glasses 1988 29 3 121-126