Glass Transition In Instant Freezing Theories - A Comparison Of Frozen-In Temper Stresses

In this article the authors give a brief summary of the theories by Adams and Williamson, Bartenev and Idenbom and discuss their numerical implementation. Frozen-in temper stresses are calculated and discussed within the model of a symmetrically cooled, infinite glass plate. Based on the numerical solution of the heat conduction equation with a given heat transfer coefficient, the influence of initial temperature of quenching is investigated.

Author
W Seifert Et Al
Origin
Martin-Luther-Universitat, Germany
Journal Title
Glastech Ber Glass Sci Technol 71 12 1998 341-351
Sector
Special Glass
Class
S 1590b

Request article (free for British Glass members)

Glass Transition In Instant Freezing Theories - A Comparison Of Frozen-In Temper Stresses
Glastech Ber Glass Sci Technol 71 12 1998 341-351
S 1590b
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 11 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.