Glass Toughening Thermometer

The Land Glass Toughening Thermometer is designed to provide both an accurate measurement at the critical toughening temperature and a fast response to changing temperatures. Within the thermometer's measurement range of 300 deg C to 800 deg C there is a high accuracy span from 625 to 650 deg C. The speed of response of the thermometer is adjustable between 150 milliseconds and three seconds. For more information please contact Land Infrared, website: www.landinst.com

Author
Un-named
Origin
Unknown
Journal Title
Glass 79 8 Sept 2002 295
Sector
News Items
Class
N 1257