Glass Tank Refractory Performance Calculated Under Extreme Manufacturing Conditions

Refractories have been traditionally used in the extreme conditions where molten glass is processed and corrosive conditions exist. A series of studies sponsored by the CGR investigated the mechanical performance of refractory structures. To understand how refractories respond under extreme conditions, calculations of the forces in walls and arches of tanks were performed. Numerical analyses of refractory materials within glass tanks are helping to identify thermo-mechanical stresses and deformations in the refractories of the glass tank. Problems such as these are important to the production of quality glass and to the safety and maintenance of the long life of the glass facility.

Author
W Carlson & M K Koyuncu
Origin
Alfred University, Usa
Journal Title
The Glass Researcher 10/2 & 11/1 2001 44-46, 54
Sector
Refractories
Class
R 397

Request article (free for British Glass members)

Glass Tank Refractory Performance Calculated Under Extreme Manufacturing Conditions
The Glass Researcher 10/2 & 11/1 2001 44-46, 54
R 397
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 7 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.