Glass Surface Corrosion And Protective Interleaving Systems

The historical development of glass interleaving systems is addressed within the context of the phenomenon of glass surface corrosion. Early 20th century investigations into the viability of using paper as a separation medium in the flat glass industry are explored in order to establish the technological foundation that that underpins the subsequent introduction of powdered materials. In addition, contemporary advances in the use of anti-corrosive interleaving materials are summarised using information gleaned from the patent literature as well as promotional brochures and information disseminated by the vendors of such materials. Finally, several examples of corrosive damage to glass will be presented in order to demonstrate the challenges that persist in maintaining surface quality during post-production storage and handling.

Author
P F Duffer
Origin
Sgcd
Journal Title
69Th Conf On Glass Problems 181-187
Sector
Flat glass
Class
F 3106

Request article (free for British Glass members)

Glass Surface Corrosion And Protective Interleaving Systems
69Th Conf On Glass Problems 181-187
F 3106
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
9 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.