Glass Surface Analysis By Secondary Ion Mass Spectroscopy

Widely used for over 20 years to characterised glass surfaces, SIMS appears to be a very powerful technique for analyzing modifications of the surface composition during all sorts of treatments, such as aging, dealkalization, diffusion - as well as for analyzing layers deposited on glass, both organic and inorganic, with a lateral resolution that can easily be in the 0.1-1um range. All elements, including those of low atomic number, can be studied on modern instruments that analyze both positively and negatively charged secondary ions. The accuracy of these analyses can be within 10-20% if sensitivity factors have been established using reference samples with compositions close to that of the unknown. Comparison with a standard is necessary for a correct interpretation.

Author
P Lehuede
Origin
Saint-Gobain Recherche
Journal Title
The Glass Researcher 9 1 1999 6, 20
Sector
Special Glass
Class
S 1776

Request article (free for British Glass members)

Glass Surface Analysis By Secondary Ion Mass Spectroscopy
The Glass Researcher 9 1 1999 6, 20
S 1776
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
10 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.