Glass As Solid Non-Equilibrium Phase Under Negative Pressure

A general condition of transformation of a liquid or a crystal into a glass according to results of measurements of specific heats and transition heats is the drop in the internal pressure to negative values.

Author
L Landa Et Al
Origin
Guardian Ind Corp, Usa
Journal Title
9Th Esg Conference, Trencin, Slovak Republic, June 2008 117-122