Glass Reycling In 2011: The Uk Situation

In 2010, more than 1.6M/tonnes of cullet was recycled in the UK, but only 600,000 tonnes of this was used by the UK glass industry. In this article, British Glass' newly appointed Head of Container Affairs, Rebecca Cocking, assesses the reasons behind the lack of cullet availability within the UK glass sector and ways in which it could be improved.