Glass Researchers At Vaxjo: We See Glass As A Winner (Swedish)

The activities of the Glasforsningsinstitut in Sweden are reviewed with particular reference to work on breakage, thickness and crack formation. The advantages of glass as a packaging material are discussed briefly.

Author
R Wehander
Origin
Unknown
Journal Title
Pack Marknaden 1987 10 24-25
Sector
Container glass
Class
C 36