Glass Research And Development In The Usa: An Overview

Some factors of competition in the American glass industry are briefly considered from a technical and economical point of view. Several examples of new processes and products are also described.

Author
T P Seward
Origin
Corning Inc., Usa
Journal Title
Riv Staz Sper Vetro 1991 21 5 229 - 235