Glass Recycling In The Netherlands

Glass recycling in the Netherlands has grown from 10,000 tonnes to 300,000 tonnes per annum. The various advantages and problems of the glass cycle with reference to the state-of-the-art in the Netherlands is described in this paper. Particular attention is given to automated sorting and sampling.