Glass & Metal Architecture Of The 19Th Century. Historical & Technological Outlines On Buildings - An Example In Venice (In Italian)

This paper analyses the characteristics of the architecture of the 19th Century made of iron and glass, pointing out the connection between constructive language and technological innovation in the productive processes of these two materials. Glassmaking is described with particular reference to blown glass.