Glass Membrane Electrodes With Solid-State Internal Contacts For Ph And Pna Measurements

The manufacture and properties of novel glass electrodes with solid-state contacts are described.

Author
W Vonau & H Kaden
Origin
Kurt-Schwabe Inst, Meinsburg, Germany
Journal Title
Glastech Ber Glass Sci Tech 70 5 1997 155-160