Glass Melting Strategies At Oberland Glass

The melting procedures adopted by Oberland are described. The main features are computer integrated manufacture, high cullet ratios and use of both filter and electrostatic precipitator methods of pollution control.

Author
W Krause
Origin
Oberland Glas Ag
Journal Title
Glass International June 1990 49, 51
Sector
Container glass