Glass Melting Process Optimisation By Statistical Methods

Glass melting process optimisation through the use of a D-optimal statistical experimental design is demonstrated.

Author
K E Washburn & D Earl
Origin
Alfred University, Usa
Journal Title
Glass Technology 44 6 2003 231-234