Glass Matrix Composite Materials With Dispersion Reinforcement. A Review - Part 1: Historical Development And Fabrication Techniques

This review covers early and current international research on the fabrication, microstructure, properties and applications of dispersion reinforced glass matrix composites. Powder technology and hot pressing are the standard processing techniques employed to fabricate these composites, however, other techniques, including sol-gel and colloidal processing have been considered.

Author
A R Boccaccini
Origin
Tech Universitat Ilmenau, Germany
Journal Title
Verre 5 2 1999 3-12
Sector
Special Glass
Class
S 1632

Request article (free for British Glass members)

Glass Matrix Composite Materials With Dispersion Reinforcement. A Review - Part 1: Historical Development And Fabrication Techniques
Verre 5 2 1999 3-12
S 1632
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
5 + 8 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.