Glass Handling In Tempering Furnaces

Fused silica rollers are widely used to convey glass in high temperature environments, the tempering furnace being among the most demanding operations. According to Gilbert Rancoule, development of SO2 injection is creating singular working conditions that influence roll operation and require understanding of the chemical reactions created.