Glass-To-Glass Modules

Advanced Solar Photonics (ASP), an American manufacturer of photovoltaic (PV) equipment and a provider of turnkey alternative energy systems, has introduced a line of glass-to-glass crystalline silicon PV modules. The dual sided glass (G2G) PV solar panels feature thinner toughened glass, which reduces the distance light travels, thereby increasing overall module efficiency by 10%. To further increase efficiency, ASP modules have a holographic material between the silicon and EVA layers, maximising the time per day they can generate electricity from the sun.

Author
Un-named
Origin
Unknown
Journal Title
Solar & Flat Glass 1 Sept/2012 4
Sector
Special Glass
Class
S 3923

Request article (free for British Glass members)

Glass-To-Glass Modules
Solar & Flat Glass 1 Sept/2012 4
S 3923
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 3 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.