Glass For Glass-Ceramic Compositions

Tests have indicated that bismuth-lead borate glasses can be recommended as suitable starting materials for the production of glass-ceramic condensers.

Author
N S Shuster Et Al
Origin
Unknown
Journal Title
Glass And Ceramics 1987 44 9-10 437-439