Glass Is Getting Smart

Glass is enhanced with added functions to form an integral part of the building network, although still in the early stages of development. This article looks at smart glass, which will be presented as a theme at glasstec 2018, which takes place in October 23-26 in Dusseldorf.

Author
Un-named
Origin
Unknown
Journal Title
Kanch 5 4 2018 41-43
Sector
General
Class
G 4667