Glass Furnace Design

A great many factors need to be taken into consideration when it comes to furnace construction - this article examines the most important.

Author
Un-named
Origin
Unknown
Journal Title
Asian Ceramics & Glass August 2001 30-33, 35
Sector
General
Class
G 2407