Glass Formation And Structure Of Non-Oxide Glasses

In this paper the characteristics of glass formation and structure of non-oxide glasses have been summarised and some basic points have been discussed.

Author
F Gan
Origin
Shangai Inst Optics & Fine Mechanics, China
Journal Title
Chimica Chronica, New Series 23 1994 295-302
Sector
Special Glass
Class