Glass Formation And Properties In The System Calcia-Gallia-Silica

The glass formation region of the calcia-gallia-silica system was determined. Measurements of density, refractive index, Abbe number, thermal expansion coefficient, softening temperature and Vickers microhardness are reported.

Author
P W Angel, C S Ray, D E Day
Origin
University Of Missouri-Rolla
Journal Title
J Am Ceram Soc 1990 73 10 2965-2969