Glass Finishing With Quality Wheels

Boosted by modern architecture, demand for float glass products has increased considerably in the past decades. Glass polishing is a very old craft, and skilled craftsmen have specialized in finishing this material ever since ancient times. The finished product, however, is very expensive and has often been limited to an exclusive clientele. In this paper, the author reviews Artifex's polishing wheels for automatic and semi-automatic machinery used in glass edge finishing operations.

Author
M Meissner
Origin
Artifex Dr. Lohmann Gmbh & Co
Journal Title
Glass-Tech Int 1/98 108-109, 111
Sector
Flat glass
Class
F 822